Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem INSPIRE™ 222 Performance Polypropylene Polymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Braskem
Trade Name INSPIRE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem INSPIRE™ 222 Performance Polypropylene Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INSPIRE™ 222 Performance Polymer is intended for use in extrusion and thermoforming processes. It is especially suited in applications requiring excellent clarity and good stiffness.Contains a nucleating agentHigh clarityComplies with Europe EU-Directive 2002/72/EC, U.S. FDA 21 CFR 177.1520(c)3.2aThis product line was spun off from Dow Chemical to Braskem
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.2 MPa
5110 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus, 1% Secant 1450 MPa
210000 psi
ASTM D790
Izod Impact, Notched 0.214 J/cm

@Temperature 0.000 °C
0.401 ft-lb/in

@Temperature 32.0 °F
ASTM D256A
0.694 J/cm

@Temperature 23.0 °C
1.30 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
DSC; Dow Method
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
234 °F
Unannealed; ASTM D648
Optical Properties Metric English Comments
Haze 2.6 %
2.6 %
254 microns; Thermoformed; ASTM D1003
21 %
21 %
1020 microns; Injection Molded; ASTM D1003