Material Notes:
HE150 resin is a high-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It has been specially designed for the monofilament extrusion process and provides a good balance of processability, spinnability, and knotting strength as well as a very low gels amount. It can also be blended with LLDPE to improve blown film stiffness. It contains processing aid and antioxidant additives. Its applications include Raschel, shading and protecting nets, and ropes.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM-D792
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM-D2240
Tensile Strength at Break 40.0 MPa
5800 psi
ASTM-D638
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM-D638
Flexural Modulus, 1% Secant 1280 MPa
186000 psi
ASTM-D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ASTM-D648
Vicat Softening Point 128 °C

@Load 1.02 kg
262 °F

@Load 2.25 lb
ASTM-D1525