Braskem H 216 HOMO Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem H 216 HOMO Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
H 216 is a high melt flow rate homopolymer with narrow molecular weight distribution. It is designed for fiber extrusion processing with high toughness fibers. H 216 exhibits excellent processability with good melt stability and toughness/impact balance. Its applications include: staple fibers and continuous filaments with high toughness and low denier; and fibers for reinforcement of asbestos-free concrete and roof tiles.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM-D792
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 230 °C
18 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM-D785
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM-D638
Elongation at Yield 9.0 %
9.0 %
ASTM-D638
Flexural Modulus, 1% Secant 1400 MPa
203000 psi
ASTM-D790
Izod Impact, Notched 0.250 J/cm
0.468 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C
138 °F
ASTM-D648
Vicat Softening Point 151 °C

@Load 1.02 kg
304 °F

@Load 2.25 lb
ASTM-D1525