Braskem H 214 HOMO Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem H 214 HOMO Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
H 214 is a high melt flow rate homopolymer with narrow molecular weight distribution. It is specially designed for fiber extrusion and nonwoven applications. This product presents excellent processability and productivity with good toughness/strain balance. Its applications include continuous filaments for high-tenacity yarns and spunbond nonwovens.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM-D792
Melt Flow 26 g/10 min

@Load 2.16 kg,
Temperature 230 °C
26 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ASTM-D785
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM-D638
Elongation at Yield 10 %
10 %
ASTM-D638
Flexural Modulus, 1% Secant 1300 MPa
189000 psi
ASTM-D790
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
216 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C
136 °F
ASTM-D648
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ASTM-D1525