Material Notes:
Description: H 107 is a ultra-high melt flow rate additivated homopolymer used for general purposes. Designed for extrusion coating. This product exhibits excellent processability, good melt stability, as well as good transparency and glossApplications: Injection of thin wall pieces; Compounds; Waterproofing of raffia bags or big-bag.Information provided by Braskem
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792A
Melt Flow 80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 37.0 MPa
5370 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
ASTM D790
Izod Impact, Notched 0.200 J/cm

@Temperature 23.0 °C
0.375 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C
135 °F
ASTM D648
Vicat Softening Point 153 °C
307 °F
-1kg; ASTM D1525