Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem Green PE SHD7255LSL Injection Molding High Density Polyethylene

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Braskem
Trade Name Green PE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem Green PE SHD7255LSL Injection Molding High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SHC7260LS-L is a high-density polyethylene, developed for the injection molding which presents high hardness and stiffness, besides low tendency to warpage. This resin has additives against the ultraviolet radiation action. The minimum biobased content of this grade is 94%, determined according to ASTM D6866.Application: Boxes for frozen food and agricultural products, industrial containers and boxes for general use, Safety Helmets, Toilet seats, Housewares, Toys, Lids, Caps &Closures, Pallets and Boxes for beverages bottles.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.954 g/cc
0.954 g/cc
ASTM D792
ESCR 100% Igepal® <= 5.0 hour

@Temperature 50.0 °C
<= 5.0 hour

@Temperature 122 °F
h/F50; Compression molded 2mm notched-plaques; ASTM D1693
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Flexural Modulus, 1% Secant 1270 MPa
184000 psi
ASTM D790
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C
165 °F
ASTM D648
Vicat Softening Point 127 °C
261 °F
10 N; ASTM D1525
Users viewing this material also viewed the following: