Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem Green PE SHC7260 Injection Molding High Density Polyethylene

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Braskem
Trade Name Green PE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem Green PE SHC7260 Injection Molding High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SHC7260 is a high-density polyethylene, developed for the injection molding which presents high hardness and stiffness, besides low tendency to warpage. The minimum biobased content of this grade is 94%, determined according to ASTM D6866. Application: Boxes for frozen food and agricultural products, industrial containers and boxes for general use, Safety Helmets, Toilet seats, Housewares, Toys, Lids, Caps &Closures, Pallets and Boxes for beverages bottles.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.959 g/cc
0.959 g/cc
ASTM D792
ESCR 100% Igepal® <= 4.0 hour

@Temperature 50.0 °C
<= 4.0 hour

@Temperature 122 °F
h/F50; Compression molded 2mm notched-plaques; ASTM D1693
Melt Flow 7.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Yield 7.5 %
7.5 %
ASTM D638
Flexural Modulus, 1% Secant 1350 MPa
196000 psi
ASTM D790
Izod Impact, Notched 0.350 J/cm
0.656 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ASTM D648
Vicat Softening Point 126 °C
259 °F
10 N; ASTM D1525