Braskem FPT350WV3 Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem FPT350WV3 Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Narrow molecular weight distribution, antistatic, nucleated, very good mold release.Applications: Suggested uses include fast-cycle injection molding, large-part injection molding, disposable drinkware.Process: Injection Molding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength 37.9 MPa
5500 psi
2 in/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
2 in/min; ASTM D638
Flexural Modulus 1.65 GPa
240 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256A