Material Notes:
Description: Excellent processability, nucleated.Applications: Suggested uses include fast-cycle injection molding and compounding.Process: Injection Molding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 65 g/10 min

@Load 2.16 kg,
Temperature 230 °C
65 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength 37.9 MPa
5500 psi
2 in/min; ASTM D638
Elongation at Yield 8.3 %
8.3 %
2 in/min; ASTM D638
Flexural Modulus 1.65 GPa
240 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 111 °C
232 °F
ASTM D648B
Users viewing this material also viewed the following: