Braskem F2523 LDPE Blown Film Extrusion Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem F2523 LDPE Blown Film Extrusion Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LDPE F2523 is a low-density polyethylene. It has good sealing characteristics, optical, and mechanical properties. It contains antiblock and slip additives. Its applications include general purpose packaging that requires good optical and mechanical properties. Recommended film thickness: 0.020-0.100mm.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM-D792
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 230 %
230 %
ASTM-D882
Film Elongation at Break, TD 930 %
930 %
ASTM-D882
Elmendorf Tear Strength TD 110 g
110 g
ASTM-D1922
Elmendorf Tear Strength, TD 4.40 g/micron
112 g/mil
ASTM-D1922
Dart Drop 2.40 g/micron
61.0 g/mil
ASTM-D1709
Dart Drop Test 60.0 g
0.132 lb
ASTM-D1709
Film Tensile Strength at Break, MD 30.0 MPa
4350 psi
ASTM-D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM-D882
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM-D1003
Gloss 110 %
110 %
Angle 60°; ASTM-D2457
Processing Properties Metric English Comments
Blow-up Ratio (BUR) 1.8 - 3.0
1.8 - 3.0
Blow Film Extrusion
Descriptive Properties Value Comments
Temperature Profile (°C) 120-170
Blow Film Extrusion