Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem Evateno® HM 150 EVA Hot Melt Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Braskem
Trade Name Evateno®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem Evateno® HM 150 EVA Hot Melt Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Evateno® HM 150 is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content, very low molecular weight, and easy crosslinkability. Evateno® HM-150 offers good compatibility with other thermoplastic and elastomeric resins, and it can be used in blends with other polyethylenes to improve the environmental stress cracking resistance (ESCR), flexibility, and fatigue resistance. It contains antioxidant additives. Its applications include: hot-melt adhesives, coating, and blends with polyethylene and injection molded parts where flexibility and environmental stress crack resistance (ESCR) are required. Hot-melt adhesives formulation presents excellent compatibility with wax, paraffins, tackifiers, polymeric blends, and blends with asphalts.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM-D1505 / ASTM-D792
ESCR 100% Igepal® >= 300 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
>= 300 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Vinyl Acetate Content 20 %
20 %
Melt Flow 150 g/10 min

@Load 2.16 kg,
Temperature 190 °C
150 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM-D2240
Hardness, Shore D 27
27
ASTM-D2240
Thermal Properties Metric English Comments
Melting Point 83.0 °C
181 °F
ASTM-D3418
Vicat Softening Point 46.0 °C

@Load 1.02 kg
115 °F

@Load 2.25 lb
ASTM-D1525