Material Notes:
Information provided by Brandenburger Isoliertechnik GmbH&Co.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
Mechanical Properties Metric English Comments
Compressive Strength 230 MPa
33400 psi
ISO 604
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1200 °C
2190 °F
Minimum Service Temperature, Air -180 °C
-292 °F