Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bostik 2124 Flexible, Long Open Time EVA Glue Stick

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Bostik
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bostik 2124 Flexible, Long Open Time EVA Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bostik 2124 Flexible, Long Open Time EVA Glue StickFlexible. Long open time for most difficult substrates.
Physical Properties Metric English Comments
Viscosity 15000 cP

@Temperature 177 °C
15000 cP

@Temperature 350 °F
Typical
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 67.8 °C
154 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Processing Properties Metric English Comments
Pot Life >= 0.50 min
>= 0.50 min
Open Time
Descriptive Properties Value Comments
Color Milky