Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue Stick

Category Polymer , Adhesive , Thermoplastic , Nylon
Manufacturer Bostik
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue StickMedium performance. Oil resistance for wood, fabric and other porous substrates primarily in woodworking assembly operation.
Physical Properties Metric English Comments
Viscosity 11500 cP

@Temperature 177 °C
11500 cP

@Temperature 350 °F
Typical
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 91.1 °C
196 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Pot Life 0.083 - 0.50 min
0.083 - 0.50 min
Open Time
Descriptive Properties Value Comments
Color Clear Amber