BorsodChem ONGRONAT T 100 TDI 100 isocyanate

Category Polymer
Manufacturer BorsodChem Rt.
Trade Name ONGRONAT
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BorsodChem ONGRONAT T 100 TDI 100 isocyanate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description of product:Appearance: At room temperature water clear liquid. Composition: The concentration 2,4-toluene-di-isocyanate is min. 97 w/w %.The product contains beside this mainly 2,6-toluene-di-isocyanate.Field of application: The highly reactive di-isocyanate chemicals are important materials used in production of PUR products.Their reactions with various polyols and auxiliary materials is utilized to obtain miscellaneous type material structures, like foams, coatings and adhesives. Through the present product manufacturer provides one of the high purity components required for such applications and quality parameters kept in an extremely narrow range of tolerance significantly contributes to exact reproducibility of formulations.Hazard listing: T+ EXTREMELY POISONOUSInformation provided by BorsodChem Rt.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Viscosity 3.0 cP

@Temperature 25.0 °C
3.0 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Melting Point 22.0 °C
71.6 °F
Chemical Properties Metric English Comments
Acid Value <= 0.0020
<= 0.0020
HCl content, w/w %; ASTM D4667
Descriptive Properties Value Comments
2,4-isomer min 97.5 w/w%
DIN 51405
Color max. 15 APHA
ISO 6271
Hydrolizable chlorine 0.005 w/w %
ASTM D4663
TDI-isomers, total min 99.5 w/w %
ASTM 4665