Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Visico™ ME4425/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer Borealis
Trade Name Visico™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Visico™ ME4425/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Visico ME4425/LE4437 is a natural, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. ME4425 is a medium-density ethylene vinylsilane copolymer that offers improved deformation resistance, toughness, and durability over conventional low-density ethylene vinylsilane copolymers. The combination of a Visico base material, ME4425, and a tin catalyst masterbatch, LE4437, provides a highly scorch retardant compound with excellent thermal stability. ME4425/LE4437 contains a patented scorch retardant additive (SRA) that increases the processing window for a moisture crosslinking compound and minimizes the tendency for premature crosslinking in the extruder ,head or die. LE4437 should be added to ME4425 directly in the extruder hopper by dry blending at a ratio of 5 parts LE4437 to 95 parts ME4425. LE4437 also provides, in addition to catalyst, a stabilization package containing suitable antioxidants, a metal passivator and a metal deactivator. Properly mixed, during the extrusion process, ME4425/LE4437 exhibits excellent thermal stability to oxidation.LE4424/LE4437 is recommended for use as insulation for low voltage control cables and power cables up to 6 kV in rating.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ME 4425; ASTM D792
0.941 g/cc
0.0340 lb/in³
LE 4437; ASTM D792
Melt Flow 0.70 g/10 min
0.70 g/10 min
ME 4425; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 18.6 MPa
>= 2700 psi
Heat Aging (7 days at 121°C); ASTM D412
20.7 MPa
3000 psi
ASTM D412
Elongation at Break <= 50 %
<= 50 %
Hot Creep Test (150°C, .2 MPa); ICEA T-28-562
315 %
315 %
Heat Aging (7 days at 121°C); ASTM D412
350 %
350 %
ASTM D412
Tensile Set <= 5.0 %
<= 5.0 %
Hot Creep Test (150°C,.2 MPa); ICE T-28-562
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 2.3

@Frequency 60 Hz
2.3

@Frequency 60 Hz
ASTM D150
Dielectric Strength >= 21.7 kV/mm
>= 550 kV/in
ASTM D149
Dissipation Factor 0.00050

@Frequency 60 Hz
0.00050

@Frequency 60 Hz
ASTM D150
Processing Properties Metric English Comments
Middle Barrel Temperature >= 170 °C
>= 338 °F
Front Barrel Temperature >= 170 °C
>= 338 °F
Die Temperature >= 185 °C
>= 365 °F
Head Temperature >= 185 °C
>= 365 °F
Users viewing this material also viewed the following: