Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Visico™ ME4425/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer Borealis
Trade Name Visico™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Visico™ ME4425/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Visico ME4425/LE4432 is a black, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. ME4425 is a medium-density ethylene vinylsilane copolymer that offers improved deformation resistance, toughness and durability over convention low-density ethylene vinylsilane copolymers. The combination of a Visico base material, ME4425, and a tin catalyst masterbatch, LE4432, provides a highly scorch retardant compound with excellent thermal stability. ME4425/LE4432 contains a patented scorch retardant additive (SRA) that increases the processing window for a moisture crosslinking compound and minimizes the tendency for premature crosslinking in the extruder, head or die.LE4424/LE4437 is recommended for use as insulation for low voltage control cables and power cables up to 6 kV in rating.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ME 4425; ASTM D792
1.05 g/cc
0.0379 lb/in³
LE 4432; ASTM D792
Melt Flow 0.70 g/10 min
0.70 g/10 min
ME 4425; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 18.6 MPa
>= 2700 psi
Heat Aging (7 days at 121°C); ASTM D412
20.7 MPa
3000 psi
ASTM D412
Elongation at Break <= 50 %
<= 50 %
Hot Creep Test (150°C, .2 MPa); ICEA T-28-562
315 %
315 %
Heat Aging (7 days at 121°C); ASTM D412
350 %
350 %
ASTM D412
Tensile Set <= 5.0 %
<= 5.0 %
Hot Creep Test (150°C,.2 MPa); ICE T-28-562
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 2.3

@Frequency 60 Hz
2.3

@Frequency 60 Hz
ASTM D150
Dielectric Strength >= 21.7 kV/mm
>= 550 kV/in
ASTM D149
Dissipation Factor 0.00050

@Frequency 60 Hz
0.00050

@Frequency 60 Hz
ASTM D150
Processing Properties Metric English Comments
Middle Barrel Temperature >= 170 °C
>= 338 °F
Front Barrel Temperature >= 170 °C
>= 338 °F
Die Temperature >= 185 °C
>= 365 °F
Head Temperature >= 185 °C
>= 365 °F