Material Notes:
LE4217 is a black crosslinkable polyethylene compound designed for track resistant power cable insulation and jacketing. APPLICATION: LE4217 contains carbon black and UV stabilizer and specifically suited for outdoor installations such as OC cables. LE4217 is suitable as a jacket or insulation, for power cables rated up to 35kV. However it is recommended that for cables rated above 12kV, that a suitable conductor shield such as LE0594 or LE0595 be used for optimum performance. Specifications: ICEA S-94-649.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
base resin; ASTM D2839
Mechanical Properties Metric English Comments
Elongation at Break >= 300 %
>= 300 %
after aging 500h, 150°C; ASTM D638
>= 360 %
>= 360 %
after xenon aging 2000h, 23°C; ASTM D2565
400 %
400 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 135 °C
275 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
ASTM D257
Dielectric Breakdown >= 3500 V
>= 3500 V
Tracking Resistance; ASTM D2303
Dissipation Factor 0.00020

@Frequency 60000 Hz
0.00020

@Frequency 60000 Hz
ASTM D150
Track Resistance >= 1.08e+6 sec
>= 1.08e+6 sec
ASTM D2132
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month