Borealis LE0315-99 Polyethylene Thermoplastic Semiconductive Compound

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Borealis
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis LE0315-99 Polyethylene Thermoplastic Semiconductive Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LE0315-99 has the same melt flow properties as the peroxide containing material. Application: LE0315-99 is used during start up of a triple-head line. It helps to use a non-peroxide containing material until stable conditions are reached. The settings should be the same as for the peroxide containing compound.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Electrical Properties Metric English Comments
Volume Resistivity 50 ohm-cm

@Temperature 23.0 °C
50 ohm-cm

@Temperature 73.4 °F
ASTM D991
90 ohm-cm

@Temperature 90.0 °C
90 ohm-cm

@Temperature 194 °F
ASTM D991
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month