Material Notes:
LE0310-99 has the same melt flow properties as the peroxide containing material. Application: LE0310-99 is used during start up of a triple-head line. It helps to use a non-peroxide-containing material until stable conditions are reached. The settings should be the same as for the peroxide containing compound.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Electrical Properties Metric English Comments
Volume Resistivity 50 ohm-cm

@Temperature 23.0 °C
50 ohm-cm

@Temperature 73.4 °F
ASTM D991
90 ohm-cm

@Temperature 90.0 °C
90 ohm-cm

@Temperature 194 °F
ASTM D991
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month