Material Notes:
Himod FT5270 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and improved optical properties. Benefits can be obtained in terms of better down gauging possibilities and improved processability. Excellent printing quality is obtained due to high clarity and better layout.Himod FT5270 is intended for applications like: Stiff, transparent shrink films with high surface gloss and lamination film/food packaging.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.927 g/cc
0.0335 lb/in³
ISO 1183
Thickness 40.0 microns
1.57 mil
Melt Flow 0.75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 300 %
300 %
ISO 527-3
Film Elongation at Break, TD 600 %
600 %
ISO 527-3
Secant Modulus, MD 0.250 GPa
36.3 ksi
ASTM D882-A
Secant Modulus, TD 0.270 GPa
39.2 ksi
ASTM D882-A
Impact 62.7
62.7
Puncture Resistance, force (N); ASTM D5748
Puncture Energy 2.40 J
1.77 ft-lb
ASTM D5748
Coefficient of Friction, Dynamic 0.50
0.50
ISO 8295
Tear Strength, Total 2.00 N
0.450 lb (f)
TD; ISO 6383/2
3.00 N
0.674 lb (f)
MD; ISO 6383/2
Dart Drop 2.50 g/micron
63.5 g/mil
ISO 7765/1
Film Tensile Strength at Break, MD 30.0 MPa
4350 psi
ISO 527-3
Film Tensile Strength at Break, TD 25.0 MPa
3630 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point >= 115 °C
>= 239 °F
ISO 11357/03
Vicat Softening Point 101 °C
214 °F
A (10N); ISO 306
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ASTM D1003
Gloss 100 %
100 %
ASTM D2457
Transmission, Visible 90 %
90 %
transparent; thickness not quantified