Material Notes:
HJ325MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. is designed for high-speed injection molding and contains nucleating and antistatic additives. The additives are optimized to provide reduced tendency for mould plate-out. This polymer is a CR (controlled rheology) grade with narrow molecular weight distribution giving low warpage. Components molded from this grade show good ejectability and combine good stiffness with good transparency and gloss, good antistatic properties and good impact strength at ambient temperatures. Applications: thin wall containers, square containers, rectangular and flat products like lids and trays, caps and closures.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ISO 2039-2
Tensile Strength, Yield 35.0 MPa
5080 psi
50mm/min; ISO 527-2
Elongation at Yield 9.0 %
9.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.65 GPa
239 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 210 - 250 °C
410 - 482 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity high