Borealis HC110BF Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis HC110BF Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HC110BF is a polypropylene homopolymer intended for injection molding and extrusion. Applications: HC110BF has been developed especially for applications like: co-extrusion applications, print lamination, metallisable film, coated film, packages for bakery products, flower packaging. HC110BF contains no slip, antiblock, antistatic additives or nucleating additivesInformation provided by Borealis AG
Physical Properties Metric English Comments
Melt Flow 3.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Flexural Modulus 1.65 GPa
239 ksi
ISO 178