Borealis Borpact™ SG930MO Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name Borpact™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borpact™ SG930MO Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borpact™ SG930MO is a random heterophasic copolymer intended for injection molding. This grade yields high transparency and deep freeze impact resistance combined with excellent flow properties. and is designed for high-speed injection molding and contains nucleating and antistatic/demolding additives. In addition, components have good gloss, very low stress whitening and excellent taste and odor properties. Products molded from this grade have an excellent balance of see-through transparency and deep freeze impact resistance. Applications: ice cream containers, crates, deep freeze boxes for food storage, bread boxes, flip top caps, and high gloss closures.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
50mm/min; ISO 527-2
Elongation at Yield 15 %
15 %
ISO 527-2
Tensile Modulus 0.850 GPa
123 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.300 J/cm²

@Temperature -20.0 °C
1.43 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C
156 °F
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 15.0 - 40.0 °C
59.0 - 104 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
minimize
Descriptive Properties Value Comments
Injection Velocity high