Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Bormed™ RF830MO Polypropylene Copolymer for Healthcare Applications

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name Bormed™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Bormed™ RF830MO Polypropylene Copolymer for Healthcare Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bormed RF830MO is a specialty modified random copolymer polypropylene with high melt flow intended for use in medical and medical related articles. Bormed RF830MO is characterized by easy processability, high transparency, high gloss, and good stiffness and impact strength.Bormed RF830MO is designed for use in devices such as syringes and needle hubs, blood and urine tubes, catheter connections, screw caps and closures, and laboratory disposable.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 28.0 MPa
4060 psi
At 50 mm/min; ASTM D638
Elongation at Yield 12 %
12 %
At 50 mm/min; ASTM D638
Tensile Modulus 1.15 GPa
167 ksi
At 1 mm/min; ASTM D638
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648