Borealis Borclear™ RF366MO Polypropylene Random Copolymer for Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name Borclear™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borclear™ RF366MO Polypropylene Random Copolymer for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borclear™ RF366MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is designed for high-speed injection molding and contains nucleating and antistatic additives. The improved processability, even at low melt temperature, allows energy savings and faster cycle time. Products originating from this grade have excellent transparency, good organoleptic properties, good balance of stiffness and impact strength at ambient temperatures. These properties, together with high gloss, make this grade excellent choice for household and packaging articles. Borclear™ RF366MO can be also used in injection stretch blow molding (ISBM). Applications: Borclear™ RF366MO is intended for injection molding applications requiring excellent transparency, including thin wall packaging, houseware containers, caps and closures, sweet-boxes, cosmetics, appliances, and baby bottles.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
50mm/min; ISO 527-2
Elongation at Yield 11 %
11 %
ISO 527-2
Tensile Modulus 1.20 GPa
174 ksi
1mm/min; ISO 527-3
Charpy Impact, Notched 0.550 J/cm²

@Temperature 23.0 °C
2.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ISO 75-2
Optical Properties Metric English Comments
Haze 4.0 %
4.0 %
1mm plaque; Borealis Method
10 %
10 %
2mm plaque; Borealis Method
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 200 - 260 °C
392 - 500 °F
Mold Temperature 30.0 - 40.0 °C
86.0 - 104 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity high