Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Borcell™ LE1120 Low Density Polyethylene for Physically Foamed Cellular Insulation

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Wire/Cable Grade
Manufacturer Borealis
Trade Name Borcell™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borcell™ LE1120 Low Density Polyethylene for Physically Foamed Cellular Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borcell LE1120 is a low density polyethylene intended for the insulation of coaxial and radio frequency communication cables.. It contains no additives and is designed to give the lowest possible attenuation by the selection of "electrically clean" feedstock. Strict cleanliness requirements are applied in production and materials handling. Borcell LE1120 is designed to be used as insulation for radio frequency cables having extra high demand on low attenuation at high frequencies. By blending weight a suitable stabilized HDPE component prior to the extrusion, in an optimum ratio for each insulation thickness, the lowest possible attenuation can be achieved. A small amount of HE1102 is recommended as nucleating agent. Using optimized-processing conditions an expansion above 80% can be expected.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ISO 1183
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ISO 868
Tensile Strength, Yield 12.20 MPa
1769 psi
ISO 527-2
Elongation at Break 500 %
500 %
ASTM D638
Electrical Properties Metric English Comments
Dielectric Constant 2.28

@Frequency 1.80e+9 Hz
2.28

@Frequency 1.80e+9 Hz
Borealis Test
2.29

@Frequency 3.90e+9 Hz
2.29

@Frequency 3.90e+9 Hz
Borealis Test
2.3

@Frequency 1e+6 Hz
2.3

@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.000040

@Frequency 1e+6 Hz
0.000040

@Frequency 1e+6 Hz
IEC 60250
0.00015

@Frequency 1.80e+9 Hz
0.00015

@Frequency 1.80e+9 Hz
Borealis Test
0.00017

@Frequency 3.90e+9 Hz
0.00017

@Frequency 3.90e+9 Hz
Borealis Test
Processing Properties Metric English Comments
Middle Barrel Temperature >= 180 °C
>= 356 °F
Front Barrel Temperature >= 150 °C
>= 302 °F
Die Temperature >= 185 °C
>= 365 °F
Head Temperature >= 185 °C
>= 365 °F