Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Borcell™ HE1346 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Borealis
Trade Name Borcell™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borcell™ HE1346 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borcell™ HE1346 is a fully formulated compound for chemical foamed telesingles. Borcell™ HE1346 is a high-density polyethylene compound containing chemical blowing agent. Applications Borcell™ HE1346 is intended for: Foam or foam-skin insulation for telephone singles with typical expansion of 35-40%. Borcell™ HE1346 meets the following material classification: ISO 1872-PE, KEGHN, 45-D006 1 and ASTM D1248 Type III, Class A, Category 4 1 The following cable material standards are met by Borcell HE1346: EN 50290-2-23, DIN VDE 0207, 2YI1. Cables manufactured with Borcell™ HE1346 using sound extrusion practice normally comply with the following cable product standards: IEC 60708 and EN 50407.1 Refers to Base ResinInformation provided by Borealis AG
Physical Properties Metric English Comments
Bulk Density 0.500 - 0.600 g/cc
0.0181 - 0.0217 lb/in³
Density 0.943 g/cc
0.0341 lb/in³
base resin; ISO 1872-2/ISO 1183
0.945 g/cc
0.0341 lb/in³
compound; ISO 1872-2/ISO 1183
Thermal Stress Crack Resistance 1.50 hour

@Temperature 105 °C
1.50 hour

@Temperature 221 °F
IEC 60811-4-2/A
Oxidative Induction Time (OIT) >= 50 min

@Temperature 200 °C
>= 50 min

@Temperature 392 °F
IEC 60811-4-2/B
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.0 MPa
1890 psi
50mm/min, expanded 35% insulation; IEC 60811-1-1
23.0 MPa
3340 psi
50mm/min; ISO 527
Elongation at Break 500 %
500 %
50mm/min, 35% expanded insulation; IEC 60811-1-1
600 %
600 %
50mm/min; ISO 527
Electrical Properties Metric English Comments
Dielectric Constant 2.33

@Frequency 1.00e+6 Hz
2.33

@Frequency 1.00e+6 Hz
IEC 60250
Dissipation Factor 0.00040

@Frequency 1.00e+6 Hz
0.00040

@Frequency 1.00e+6 Hz
IEC 60250
Processing Properties Metric English Comments
Processing Temperature 110 - 140 °C
230 - 284 °F
conductor preheating temperature
Zone 1 155 °C
311 °F
Zone 2 170 °C
338 °F
Zone 3 185 °C
365 °F
Zone 4 195 °C
383 °F
Die Temperature 195 °C
383 °F
Die Cooling Temperature 50.0 °C
122 °F
cooling water
Descriptive Properties Value Comments
Petroleum Jelly Absorption (%) 10
IEC 60811-4-2