Borealis BorECO™ BA415E Polypropylene Block Copolymer for Non-Pressure Pipes

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name BorECO™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorECO™ BA415E Polypropylene Block Copolymer for Non-Pressure Pipes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BorECO™ BA415E is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength. This material has been designed for improved processability and higher output, especially in the production of corrugated pipes. Applications: BorECO™ BA415E is recommended for corrugated and solid wall gravity pipes, profiles, fittings and chambers in the application field of: underground drainage, sewerage, soil, and waste.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
50mm/min; ISO 527-2
Elongation at Yield 10 %
10 %
50mm/min; ISO 527-2
Flexural Modulus 1.50 GPa
218 ksi
1mm/min; ISO 178
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Processing Properties Metric English Comments
Middle Barrel Temperature 200 - 220 °C
392 - 428 °F
cylinder
Die Temperature 210 - 220 °C
410 - 428 °F
Melt Temperature 210 - 230 °C
410 - 446 °F
Head Temperature 210 - 220 °C
410 - 428 °F