Material Notes:
BJ356MO is a heterophasic copolymer. This grade provides very high melt flow rate, very high stiffness and medium impact strength. and is designed for high-speed injection molding and contains nucleating and antistatic/demolding additives. Components molded from this grade show good ejectability and combine excellent stiffness with very good gloss, good antistatic and excellent organoleptic properties. Applications: thin wall containers, household applications, and technical parts.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.906 g/cc
0.0327 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 100 g/10 min

@Load 2.16 kg,
Temperature 230 °C
100 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ISO 2309-2
Tensile Strength, Yield 29.0 MPa
4210 psi
50mm/min; ISO 527-2
Elongation at Yield 4.0 %
4.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.65 GPa
239 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.250 J/cm²

@Temperature -20.0 °C
1.19 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Puncture Energy 10.0 J

@Temperature 0.000 °C
7.38 ft-lb

@Temperature 32.0 °F
ISO 6603-2
10.0 J

@Temperature -20.0 °C
7.38 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 210 - 260 °C
410 - 500 °F
Mold Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity highest possible