Borealis BE375MO Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BE375MO Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BE375MO is a heterophasic copolymer. This grade is characterized by optimum combination of high impact strength and stiffness. This grade is formulated for an excellent antistatic performance. Electrostatic charge is
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 86
86
ISO 2309-2
Tensile Strength, Yield 26.0 MPa
3770 psi
50mm/min; ISO 527-2
Elongation at Yield 6.0 %
6.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.40 GPa
203 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Puncture Energy 25.0 J

@Temperature -20.0 °C
18.4 ft-lb

@Temperature -4.00 °F
ISO 6603-2
35.0 J

@Temperature 0.000 °C
25.8 ft-lb

@Temperature 32.0 °F
ISO 6603-2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C
208 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 210 - 260 °C
410 - 500 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity highest possible