Material Notes:
BC142MO is a controlled rheology polypropylene heterophasic copolymer. It is characterized by high impact strength, good stiffness, excellent process ability, good flow properties and low warpage. Applications: crates and boxes, and technical parts.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ISO 2039-2
Tensile Strength, Yield 25.0 MPa
3630 psi
50mm/min; ISO 527-2
Elongation at Yield 9.5 %
9.5 %
50mm/min; ISO 527
Tensile Modulus 1.10 GPa
160 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.900 J/cm²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Puncture Energy 30.0 J

@Temperature 0.000 °C
22.1 ft-lb

@Temperature 32.0 °F
ISO 6603-2
32.0 J

@Temperature -20.0 °C
23.6 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 230 - 260 °C
446 - 500 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity high