Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis BA390TF Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BA390TF Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BA390TF is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA390TF is recommended for foam extrusion, or thermoforming.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
50mm/min; ISO 527-2
Elongation at Yield 6.0 %
6.0 %
50mm/min; ISO 527-2
Flexural Modulus 1.30 GPa
189 ksi
2mm/min; ISO 178
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 163 °C
325 °F
DSC; ISO 3146
Vicat Softening Point 147 °C

@Load 1.02 kg
297 °F

@Load 2.25 lb
ISO 306
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month