Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bohler-Uddeholm UDDEHOLM VANADIS 10 SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel

Category Metal , Ferrous Metal , Alloy Steel , Tool Steel , Cold Work Steel
Manufacturer Bohler-Uddeholm
Trade Name UDDEHOLM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bohler-Uddeholm UDDEHOLM VANADIS 10 SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chromium-molybdenum-vanadium alloyed steelUddeholm Vanadis 10 is a high vanadium alloyed powder metallurgy tool steel offering a unique combination of an excellent abrasive wear resistance in combination with a good chipping resistance. It is manufactured according to the powder metallurgy process giving a very low amount of non-metallic inclusionsVanadis 10 is characterized by: Extremely high abrasive wear resistance High compressive strength Very good through hardening properties Good toughness Very good stability in hardening Good resistance to tempering backApplications: Uddeholm Vanadis 10 is especially suitable for very long run tooling where abrasive wear is the dominating problem. Its very good combination of extremely high wear resistance and good toughness also make Uddeholm Vanadis 10 an interesting alternative in applications where tooling made of such materials as cemented carbide tends to chip or crack.
Physical Properties Metric English Comments
Density 7.42 g/cc
0.268 lb/in³
hardened to 62 HRC
Mechanical Properties Metric English Comments
Hardness, Brinell 280 - 310
280 - 310
Soft annealed (Delivery condition)
Modulus of Elasticity 220 GPa
31900 ksi
(hardened to 62 HRC)
200 GPa

@Temperature 399 °C
29000 ksi

@Temperature 750 °F
hardened to 62 HRC
210 GPa

@Temperature 199 °C
30400 ksi

@Temperature 390 °F
hardened to 62 HRC
Impact Test 16.3 - 32.5 J
12.0 - 24.0 ft-lb
Tempered at 390-1110°F (2 + 2h)
Thermal Properties Metric English Comments
CTE, linear 10.8 µm/m-°C

@Temperature 199 °C
6.00 µin/in-°F

@Temperature 390 °F
hardened to 62 HRC
11.3 µm/m-°C

@Temperature 399 °C
6.30 µin/in-°F

@Temperature 750 °F
hardened to 62 HRC
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
hardened to 62 HRC
Thermal Conductivity 20.0 W/m-K

@Temperature 199 °C
139 BTU-in/hr-ft²-°F

@Temperature 390 °F
hardened to 62 HRC
22.0 W/m-K

@Temperature 399 °C
153 BTU-in/hr-ft²-°F

@Temperature 750 °F
hardened to 62 HRC
Component Elements Properties Metric English Comments
Carbon, C 2.9 %
2.9 %
Chromium, Cr 8.0 %
8.0 %
Manganese, Mn 0.50 %
0.50 %
Molybdenum, Mo 1.5 %
1.5 %
Silicon, Si 0.50 %
0.50 %
Vanadium, V 9.8 %
9.8 %
Descriptive Properties Value Comments
Pin-On-Disc wear 81 mg/min
62HRC
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved