Bohler-Uddeholm BÖHLER S500(m42) High Speed Steel

Category Metal , Ferrous Metal , Tool Steel
Manufacturer Bohler-Uddeholm
Trade Name BÖHLER
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bohler-Uddeholm BÖHLER S500(m42) High Speed Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Cobalt Molybdenum high speed steel processing high hardness, excellent cutting properties, high red hardness and good toughness. BOHLER S500 is also available in the special grade ISORAPID for heavy duty. Applications: Milling cutters, taps, twist drills, broaches tools, and cold work tools.Standards: DIN/EN 1.3346 HS2-91, AISI M1, UNS T11301, BS ~BM1
Physical Properties Metric English Comments
Density 8.10 g/cc
0.293 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 220 GPa
31900 ksi
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 100 °C
6.11 µin/in-°F

@Temperature 212 °F
11.5 µm/m-°C

@Temperature 200 °C
6.39 µin/in-°F

@Temperature 392 °F
11.9 µm/m-°C

@Temperature 300 °C
6.61 µin/in-°F

@Temperature 572 °F
12.3 µm/m-°C

@Temperature 400 °C
6.83 µin/in-°F

@Temperature 752 °F
12.4 µm/m-°C

@Temperature 500 °C
6.89 µin/in-°F

@Temperature 932 °F
12.5 µm/m-°C

@Temperature 600 °C
6.94 µin/in-°F

@Temperature 1110 °F
12.5 µm/m-°C

@Temperature 700 °C
6.94 µin/in-°F

@Temperature 1290 °F
Specific Heat Capacity 0.431 J/g-°C
0.103 BTU/lb-°F
Thermal Conductivity 20.0 W/m-K
139 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C 1.1 %
1.1 %
Chromium, Cr 3.9 %
3.9 %
Cobalt, Co 7.8 %
7.8 %
Iron, Fe 74.9 %
74.9 %
As remainder
Manganese, Mn 0.20 %
0.20 %
Molybdenum, Mo 9.2 %
9.2 %
Silicon, Si 0.50 %
0.50 %
Tungsten, W 1.4 %
1.4 %
Vanadium, V 1.0 %
1.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000520 ohm-cm
0.0000520 ohm-cm