Bohler-Uddeholm BÖHLER S401(M1) High Speed Steel

Category Metal , Ferrous Metal , Tool Steel
Manufacturer Bohler-Uddeholm
Trade Name BÖHLER
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bohler-Uddeholm BÖHLER S401(M1) High Speed Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Molybdenum high speed steel with high toughness and good cutting ability. Applications: Taps, twist drills, reamers, milling tools, broaches toolsStandards: DIN/EN 1.3346 HS2-91, AISI M1, UNS T11301, BS ~BM1
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 217 GPa
31500 ksi
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 100 °C
6.11 µin/in-°F

@Temperature 212 °F
11.5 µm/m-°C

@Temperature 200 °C
6.39 µin/in-°F

@Temperature 392 °F
11.9 µm/m-°C

@Temperature 300 °C
6.61 µin/in-°F

@Temperature 572 °F
12.3 µm/m-°C

@Temperature 400 °C
6.83 µin/in-°F

@Temperature 752 °F
12.4 µm/m-°C

@Temperature 500 °C
6.89 µin/in-°F

@Temperature 932 °F
12.5 µm/m-°C

@Temperature 600 °C
6.94 µin/in-°F

@Temperature 1110 °F
12.5 µm/m-°C

@Temperature 700 °C
6.94 µin/in-°F

@Temperature 1290 °F
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Thermal Conductivity 19.0 W/m-K
132 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C 0.84 %
0.84 %
Chromium, Cr 3.8 %
3.8 %
Iron, Fe 83.06 %
83.06 %
As remainder
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 8.6 %
8.6 %
Silicon, Si 0.40 %
0.40 %
Tungsten, W 1.8 %
1.8 %
Vanadium, V 1.2 %
1.2 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000600 ohm-cm
0.0000600 ohm-cm