Material Notes:
BLUE RIVER COATINGS Semi-Transparent Wood Stain is a water based stain developed to provide long lasting protection and a beautiful appearance on wood surfaces. BLUE RIVER COATINGS Semi-Transparent Wood Stain offers the advantages of deep penetrating pigments and excellent moisture repellency. The product dries quickly, therefore minimizing excessive grain raise. The product can be used as an interior or exterior stain.Enviromental Advantages:BLUE RIVER COATINGS Semi-Transparent Wood Stain is a low VOC (Volatile Organic Compound), high performance stain product. It is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with your local and state regulations for proper handling. Characteristics:Interior or exterior applicationExcellent pigment penetrationMinimal grain raisingCan be applied in a wide variety of temperature and humidity conditionsWater is used for clean-upNon-HazardousShelf life of 1 yearNon-FlammableUsesRedwoodPineCedarFirPressure Treated LumbarDecksFencesShake ShinglesLog HomesAny wood surface that can be stainedInformation provided by Blue River Coatings
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
Density 1.02 g/cc
0.0368 lb/in³
Solids Content 17.3 %
17.3 %
by volume
22.4 %
22.4 %
by weight
Volatile Organic Compounds (VOC) Content 60 g/l
60 g/l
Thermal Properties Metric English Comments
Boiling Point 169 °C
336 °F
Flash Point 65.6 °C
150 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 140 °C
0.0500 hour

@Temperature 284 °F
Dry to stack, at 50% humidity
4.98 min

@Temperature 75.0 °C
0.0830 hour

@Temperature 167 °F
Dust Free, at 50% humidity
4.98 min

@Temperature 75.0 °C
0.0830 hour

@Temperature 167 °F
Recoat, at 50% humidity
10.0 min

@Temperature 75.0 °C
0.167 hour

@Temperature 167 °F
Dry to handle, at 50% humidity and 75°C
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesion Excellent; pressure treated wood
Theoretical Coverage 277 ft2 at 1 mil