Material Notes:
A through hardened, abrasion resistant steel plate, offering long life expectancy in sliding and gouging abrasion applications.Applications: Dump Truck Wear Liners, Chutes, Wear Liners, Earth Moving Buckets, Ground Engaging Tools, Cutting EdgesWelding: According to AS/NZS 1554 parts 4 and 5Tolerance: In accordance with AS/NZS 1365
Mechanical Properties Metric English Comments
Hardness, Brinell 500
500
Tensile Strength at Break 1640 MPa
238000 psi
Tensile Strength, Yield 1400 MPa

@Strain 0.200 %
203000 psi

@Strain 0.200 %
Elongation at Break 10 %
10 %
in 50 mm GL
Charpy Impact 35.0 J
25.8 ft-lb
Longitudinal, (10mmx10mm)
Component Elements Properties Metric English Comments
Boron, B 0.0010 %
0.0010 %
Carbon, C 0.29 %
0.29 %
Chromium, Cr 1.0 %
1.0 %
Iron, Fe 97.6 %
97.6 %
As Balance
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 0.25 %
0.25 %
Nickel, Ni 0.20 %
0.20 %
Phosphorous, P 0.015 %
0.015 %
Silicon, Si 0.30 %
0.30 %
Sulfur, S 0.0030 %
0.0030 %
Descriptive Properties Value Comments
CE (IIW) 0.61
PCM 0.4
Surface Finish Shotblasted