Beijing Ranger Chem SM-828CA Liquid Epoxy Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Beijing Ranger Chemical Co
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Ranger Chem SM-828CA Liquid Epoxy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Beijing Ranger Chemical Co.
Physical Properties Metric English Comments
Viscosity 12000 - 15000 cP
12000 - 15000 cP
Descriptive Properties Value Comments
Color APHA,= 50
Epoxy Equivalent g/eq 200-230
Saponifiable Chlorine ppm, = 1.8-2.1%