Beijing Ranger Chem E-42B Semi Solid Epoxy Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Beijing Ranger Chemical Co
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Ranger Chem E-42B Semi Solid Epoxy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Beijing Ranger Chemical Co.
Thermal Properties Metric English Comments
Softening Point 30.0 - 38.0 °C
86.0 - 100 °F
Descriptive Properties Value Comments
Epoxy Equivalent g/eq 238-286