Beijing Evergrow Resources UHMW PE Sheet

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Beijing Evergrow Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources UHMW PE Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultra-high molecular weight polyethylene (UHMWPE) is an outstanding engineering plastic. It’s characterized by the following properties.Features:Very high abrasion resistanceVery high impact strengthVery low coefficient frictionGood self-lubricantExcellent resistance to chemicalsGood resistance to low temperatureExcellent dielectric propertiesApplications:Abrasion Resistance and Self-lubricant : marine fender, truck liners, gearing wheels, bearing bushes, sliding elements, chute liners, bunker liners, chain wear strip, guide strips and liners. paper and cardboard Industry, suction blades, foil blades, scraper and deflecting blades etc.Excellent Impact Strength : lug straps, picker stickers, loom pickers, picker shields and spinning etc.Hygienically : food processing, slide guide mechanisms, cutting boards, rammers, rolling pins, chopping blocks and moulds etc.High Resistance to Chemical Solvents: pump casings, seals, spray nozzles, agitator screws, acid pump impellers and valve liners, electroplating plating drums etc.Information provided by Beijing Evergrow Resources.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 24.0 MPa
>= 3480 psi
Elongation at Break >= 140 %
>= 140 %