Beijing Evergrow Resources PTFE Tube and Pipe

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Extruded
Manufacturer Beijing Evergrow Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources PTFE Tube and Pipe.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PTFE tubing is manufactured by ram extruding method with PTFE granular resin. It has good electrical properties.Information provided by Beijing Evergrow Resources.
Physical Properties Metric English Comments
Density 2.10 - 2.30 g/cc
0.0759 - 0.0831 lb/in³
apparent
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 18.0 MPa
>= 2610 psi
Elongation at Break >= 230 %
>= 230 %