Material Notes:
Information provided by Beijing Evergrow Resources.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
GB1033
Mechanical Properties Metric English Comments
Hardness, Shore D 80 - 85
80 - 85
GB3398
Ball Indentation Hardness 142.4 MPa
20650 psi
GB3398
Tensile Strength at Break 69.5 MPa
10100 psi
GB/T 1040
Elongation at Yield 22 %
22 %
GB/T 1040
Modulus of Elasticity 3.30 GPa
479 ksi
GB/T 1040
Flexural Strength 86.9 MPa
12600 psi
GB9341
Compressive Strength 85.0 - 100 MPa
12300 - 14500 psi
GB/T 1040
Izod Impact, Notched (ISO) 9.60 kJ/m²
4.57 ft-lb/in²
GBT1043
Coefficient of Friction 0.131
0.131
GB3360
Thermal Properties Metric English Comments
CTE, linear 75.0 µm/m-°C
41.7 µin/in-°F
GB1036
Melting Point 223 °C
433 °F
HG/T2235
Heat Distortion Temperature 120 °C
248 °F
GB1634
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Volume; GB1410
Arc Resistance 600 sec
600 sec
ASTM D112
Processing Properties Metric English Comments
Moisture Content 2.0 - 2.2 %
2.0 - 2.2 %
in air
6.6 - 6.8 %
6.6 - 6.8 %
in water