Material Notes:
BVC 6200-85 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a smooth semi-gloss finish. Typical applications are wire coating, weather stripping, tubing, profiles and a variety of injection molded items.Information Provided by Bayshore Vinyl Compounds Inc.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85

@Time 10.0 sec
85

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 13.8 MPa
2000 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
100% Modulus 0.00758 GPa
1.10 ksi
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -23.0 °C
-9.40 °F
Impact Brittleness; ASTM D746
Copyright © lookpolymers.com All Rights Reserved