Barlog Plastics KEBATER BFA30 PBT, 30% glass fiber reinforced, flame retardant

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
Manufacturer Barlog Plastics
Trade Name KEBATER
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBATER BFA30 PBT, 30% glass fiber reinforced, flame retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PBT-GF30 FRInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.15 %
0.15 %
similar to ISO 62 test
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ISO 527-1
Elongation at Break 3.0 %
3.0 %
ISO 527-1
Tensile Modulus 10.5 GPa
1520 ksi
ISO 527-1
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179-1eU
Charpy Impact, Notched 1.05 J/cm²
5.00 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
22.2 µin/in-°F
ISO 11359-1/-2
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 208 °C
406 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
UL Registered; IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Descriptive Properties Value Comments
Resin Type PBT-GF30 FR