Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Barlog Plastics KEBATER B512A PBT unreinforced, flame retardant

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer Barlog Plastics
Trade Name KEBATER
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBATER B512A PBT unreinforced, flame retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PBT FR(17)Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.20 %
0.20 %
similar to ISO 62 test
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527-1
Elongation at Break 12 %
12 %
ISO 527-1
Tensile Modulus 2.05 GPa
297 ksi
ISO 527-1
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179-1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched 0.950 J/cm²
4.52 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
UL Registered; IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Descriptive Properties Value Comments
Resin Type PBT FR(17)
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved