Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy + GF , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Barlog Plastics
Trade Name KEBATER
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBATER A0130 PBT/ABS, 30% glass fiber reinforced, low warpage.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
(PBT+ABS)-GF30Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ISO 527-1
Elongation at Break 2.5 %
2.5 %
ISO 527-1
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527-1
Charpy Impact Unnotched 5.50 J/cm²
26.2 ft-lb/in²
ISO 179-1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Descriptive Properties Value Comments
Resin Type (PBT+ABS)-GF30