Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Barlog Plastics KEBAFORM C 906 UR POM Copolymer unreinforced, impact modified

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Impact Modified
Manufacturer Barlog Plastics
Trade Name KEBAFORM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFORM C 906 UR POM Copolymer unreinforced, impact modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POM-IInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO 294-4
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO 527-1
Elongation at Yield 20 %
20 %
ISO 527-1
Tensile Modulus 1.30 GPa
189 ksi
ISO 527-1
Charpy Impact Unnotched NB
NB
ISO 179-1eU
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Descriptive Properties Value Comments
Resin Type POM-I
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved