Barlog Plastics KEBAFORM C 3090(K) POM Copolymer, 27% glass fiber reinforced

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 30% Glass Fiber Reinforced
Manufacturer Barlog Plastics
Trade Name KEBAFORM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFORM C 3090(K) POM Copolymer, 27% glass fiber reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POM-GF27Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.15 %
0.15 %
similar to ISO 62 test
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ISO 527-1
Elongation at Break 1.8 %
1.8 %
ISO 527-1
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527-1
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 164 °C
327 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Resin Type POM-GF27
Users viewing this material also viewed the following: