Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Barlog Plastics KEBAFLEX U A 85 ST B01 natural TPU, Shore A85, natural

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Barlog Plastics
Trade Name KEBAFLEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFLEX U A 85 ST B01 natural TPU, Shore A85, natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPUInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
Tensile Strength at Break 45.0 MPa
6530 psi
ISO 527-1
Elongation at Break 750 %
750 %
ISO 527-1
Charpy Impact, Notched NB
NB
ISO 179-1eA
Descriptive Properties Value Comments
Resin Type TPU
Copyright © lookpolymers.com All Rights Reserved